25 lbs
△5/6
Plastic clay for wheel and modeling. Granular manganese gives speckled surface. Ideal temperature for best color is C/5. Good in oxidation or reduction firing.
Fired Shrinkage is 11% and Water Absorption is 2.25% when fired to cone 5.
25 lbs
△5/6
Plastic clay for wheel and modeling. Granular manganese gives speckled surface. Ideal temperature for best color is C/5. Good in oxidation or reduction firing.
Fired Shrinkage is 11% and Water Absorption is 2.25% when fired to cone 5.