C/4-C/6
Plastic clay for wheel and modeling. Granular manganese gives speckled surface. Ideal temperature for best color is C/5. Good in oxidation or reduction firing.
Contains manganese.
C/6 Average Shrinkage 11.0% Absorption 2.25%
C/4-C/6
Plastic clay for wheel and modeling. Granular manganese gives speckled surface. Ideal temperature for best color is C/5. Good in oxidation or reduction firing.
Contains manganese.
C/6 Average Shrinkage 11.0% Absorption 2.25%